ISO 16770 – Full-Notch Creep Test (FNCT)

0 out of 5

ISO 16770 specifies a method of determining the stress cracking resistance of polyethylene materials in any environment.

Please Contact With Us For More Information

Description

Description

ISO 16770 – Plastics — Determination of Environmental Stress Cracking (ESC) of Polyethylene 

Full-Notch Creep Test (FNCT)

 

ISO 16770 specifies a method of determining the stress cracking resistance of polyethylene materials in any environment.

The test is carried out on notched test specimens cut from compression-moulded sheet or finished products, as applicable.

The test specimen is subjected to a static tensile load when immersed in an environment such as a surfactant solution held at a specified temperature, and the time

to failure measured.

The method has been specifically developed for polyethylene materials but can be used to evaluate PE extrusions, such as pipe segments, PE fusion welds/fittings

and blow-moulded PE containers to study the effect of aggressive environments, i.e. dangerous goods/chemicals.

The method may also be adapted for other thermoplastic materials, e.g. polypropylene (PP).

In this case, care must be taken in interpreting the results as the processing stresses/orientation in finished products may have an effect.

*** Before conducting ISO 16770 , it is important to read the entire specification. Standards can be obtained from appropriate standard authorities.

 

***PARSROS  offers several types of grips and fixtures which will enable you to perform a variety of tests

  that are accurate and repeatable.

TECHNICAL SPECIFICATIONS

Please Contact  with our engineers so that we can find and offer  Best Universal Tensile Test Machines , Grips , Jaws and Other Accessories for your operations